The company is proficient in various Cobalt Based Alloy Powder, Flake Silver Powder, 316L Stainless Steel Powder processing techniques and has a professional technical team. The company insists on win-win cooperation, guarantees the interests of customers, and looks forward to common development with customers to create a better future. Our company adheres to the core values of 'innovation and change, dedication, moderate competition, and excellent team'. We provide customers with safe, reliable, efficient and economical products accurately and quickly according to customer needs.
Our main business:Metal powder,Electronic paste,Brazing materials,3D printing/VIGA equipment,R&D production and sales of customized products.
7x24 hours delivery
7x24 hours delivery capacity,is the best partner for enterprise globalization

3
VIGA Lines
1
Water&Gas Atomizer Line
1
Plasma Atomizer Line
236M
Projects Completed
Hunan Mana Materials Technology Co.,Ltd. is located in Changsha city,Hunan province,China ,which is the hometown of non-ferrous metals.Mana is a technology enterprise focusing on the research and development,production and sales of new materials.At present, the main products on sale include electronic paste, metal powders, brazing materials,3D printing/VIGA equipment,R&D production and sales of customized products. With more than ten years of metal powder manufaturing technology and experience, we provide highly competitive high-quality products.

01
High Quality
02
Advanced Equipment
03
Professional Team
04
Custom Service
Inconel 718 (IN718) is a well-known nickel-based superalloy that is extensively used in high-value-added engineering applications such as jet engines in aerospace and steam generators in nuclear power plants, as well as in the defense and marine sectors. It has excellent mechanical properties, fatigue resistance, and corrosion resistance.

01
Powder characteristics
Powder characteristics: high batch stability, good sphericity, low oxygen content, uniform particle size distribution, good fluidity, high bulk density and tap density.
02
Applicable processes
Powder can be used for laser/electron beam additive manufacturing (SLM/EBM), powder metallurgy (PM), laser direct deposition (DLD), powder hot isostatic pressing (HIP), metal injection molding (MIM) and other processes.
03
Applicable equipment
Powder can be used for various types of metal 3D printers, including Renishaw in the UK, EOS, ConceptLaser in Germany, SLM, 3D systems in the United States, Arcam, BLT, Farsoon, E-Plus, HBD, etc.
04
Powder application
Nickel-based metal powder is widely used in industrial and aviation turbines, petrochemicals, nuclear reactors, laser cladding and other fields.
Product Specification
|
Norminal Composition(wt%) |
||||||
|
In718 |
Cr |
Mo |
Nb |
Co |
Fe |
Al |
|
17.0-21.0 |
2.8-3.3 |
4.75-5.5 |
≤1 |
Bal. |
0.2-0.8 |
|
|
Ti |
Si |
Ni |
O |
N |
||
|
0.65-1.15 |
≤0.35 |
50-55 |
≤500ppm |
≤100ppm |
||
Common Size:15-45um,15-53um,45-106um,45-150u,-200/-300/-400/-500/-600mesh etc,.
|
No |
Name |
Chemical Composition(wt%) |
|
1 |
18Ni300 |
Ni17-19,Mo4.5-5.2,Co8.5-9.5,Ti0.6-0.8,Al0.05-0.15,Fe(Bal.) |
|
2 |
Hastelloy Alloy |
Fe17-20,Cr20.5-23,Mo8-10,W0.2-1,Co0.5-2.5,C0.05-0.15,Ni(Bal.) |
|
3 |
AlSi10Mg |
Si9-11,Mg0.2-0.45,Al(Bal.) |
|
4 |
CoCrW |
Cr26.5-29,W7-9,Si1.2-1.9,Co(Bal.) |
|
5 |
Co28Cr6Mo |
Cr27-29,Mo5-7,Co(Bal.) |
|
6 |
Spherical Ti Powder |
Ti≥99.9 |
|
7 |
TC4 |
Al5.5-6.8,V3.5-4.5,Ti(Bal.) |
|
8 |
TA15 |
Al5.5-7.1,V0.8-2.5,Mo0.8-2,Zr1.5-2.5,Al(Bal.) |
|
9 |
316L |
Cr16.00-18.00, Ni10.00-14.00,Mo2.00-3.00,Fe(Bal.) |
|
10 |
S136 |
Cr12.0-14.0,Si0.8-1.0,V0.15-0.4,C0.2-0.45,Fe(Bal.) |
|
11 |
In625 |
Cr20-23 , Mo8-10 , Nb 3.15-4.15 , Co≤1, Fe≤1 , Ni (bal.) |
|
12 |
In718 |
Cr17-21 , Mo2.8-3.3 , Nb 4.75-5.5 , Co≤1, Ni50-51 , Fe(Bal.) |
|
13 |
Spherica WC |
C3.7-4.2,W(Bal.) |
|
14 |
Spherical Cr Powder |
Cr≥99.9 |
|
15 |
Spherica Mo Powder |
Mo≥99.9 |
|
16 |
Spherica Ta Powder |
Ta≥99.9 |
|
17 |
Spherica W Powder |
W≥99.9 |
machanical properties
Tensile Strength/MPa
1000–1100
Yield Strength/MPa
700–780
Elongation After Break/%
18–26
Tensile Strength(650℃)/MPa
1050–1180
Yield Strength(650℃)/MPa
780–860
Elongation After Break(650℃)/%
22–30
1. Appearance:Grey spherical powder
2. Tapping Density:4.89g/cm3
3. Apparent density: 4.18g/cm3
4. Flowability:18.1s/50g
5. Size: 15-53um
6. PSD: D10:23.18um, D50:35.68um, D90: 54.62um

Application

Additive manufacturing

Powder metallurgy(PM)

Metal injection moldinb(MIM)
Our Testing Equipment






Our factory & quipment






Our factory & Office



Certifications






Our Packing




FAQ
1. Who Are We?
We are based in Hunan, China, our product sell to Asia, Europe, America, North America and Southeast Asia, and we are fully capable of undertaking global business. There are total about 101-200 people in our factory
2. How Can We Guarantee Quality?
Always a pre-production sample before mass production;
Always final Inspection before shipment;
3. What Can You Buy From Us?
3D printing metal powder ,MIM powder, Brazing powder&paste, Electronic paste, the products included are 316L,17-4ph,H13,FeSiAl,Inconel718,Inconel625, Silver based filler metal, Copper based filler metal, Nickel based filler metal, Silver paste,Rare earth products.
4. Why Should You Buy From Us Not From Other Suppliers?
Hunan Mana Materials Technology Co.,Ltd is a professional manufacture metal powder and paste .High purity rare earth series and other products etc. We have factory. We are sure we can supply the high quality products with competitve price.
5. What Services Can We Provide?
Accepted Delivery Terms: FOB,CIF,EXW,DDP,DDU,Express Delivery;
Accepted Payment Currency:USD,RMB
Accepted Payment Type: T/T,Paypal
Language Spoken:English,Chinese
Hot Tags: cuzn45 brazing filler metal, China, suppliers, factory, customized, price, cheap, for coating, for 3D printing, Silver Based Brazing Alloy, CuSnTi Brazing Filler Metal, CuP8 Brazing Filler Metal, Silver Based Brazing Alloy, CuSnTi Brazing Filler Metal, CuP8 Brazing Filler Metal
We are committed to becoming the most respected company in the industry and insist on providing customers with more Superflow Superalloy Spherical Powder Inconel718/625/Gh3536 for 3D Printing with corporate characteristics. We attach great importance to the introduction, reserve and training strategy of talents. We believe that good business relationships will lead to mutual benefits and improvement for both parties.
Hot Tags: inconel 718 powder, China, suppliers, factory, customized, price, cheap, for coating, for 3D printing, Titanium Alloy Spherical Powder Ti-6al-4v (TC4)for 3D Printing (15-53um), 17-4PH Stainless Steel Metal Powder for MIM, Silver Powder, 440C Stainless Steel Powder, Stainless Steel Powder, Coating Powder
[[ProKeywords]]