yang@mana-metal.com    +8617871989276
Cont

Have any Questions?

+8617871989276

Additive manufacturing nickel-based superalloy IN718 powder GH4169 powder Inconel718 powder

Additive manufacturing nickel-based superalloy IN718 powder GH4169 powder Inconel718 powder

Inconel 718 (IN718) is a well-known nickel-based superalloy that is extensively used in high-value-added engineering applications such as jet engines in aerospace and steam generators in nuclear power plants, as well as in the defense and marine sectors.
Send Inquiry

Product Introduction

We have been ISO9001, CE, and GS certified and strictly adhere to their excellent specifications for 316L Stainless Steel Powder for MIM, Silver Paste for Piezoelectric Ceramics, Copper Based Brazing Alloy. In the new century full of opportunities and challenges, we will continue to carry forward the enterprise spirit of "diligence, rigor, harmony and innovation". We fully implement the development strategy of "value-led, innovation-driven, resource co-ordination, openness and cooperation, green and low-carbon". Brand must be another name for improving the quality, the concentration of customer satisfaction and the result of the recognition of the majority of users.

Hunan Mana Materials Technology Co.,Ltd

Our main business:Metal powder,Electronic paste,Brazing materials,3D printing/VIGA equipment,R&D production and sales of customized products.

 

7x24 hours delivery

7x24 hours delivery capacity,is the best partner for enterprise globalization

20240619111039

3

VIGA Lines

1

Water&Gas Atomizer Line

1

Plasma Atomizer Line

236M

Projects Completed

 

Company profile
 

Hunan Mana Materials Technology Co.,Ltd. is located in Changsha city,Hunan province,China ,which is the hometown of non-ferrous metals.Mana is a technology enterprise focusing on the research and development,production and sales of new materials.At present, the main products on sale include electronic paste, metal powders, brazing materials,3D printing/VIGA equipment,R&D production and sales of customized products. With more than ten years of metal powder manufaturing technology and experience, we provide highly competitive high-quality products.

20240619111312

01

High Quality

 

02

Advanced Equipment

 

03

Professional Team

 

04

Custom Service

 

 

 

 

Inconel 718 Powder
 

Inconel 718 (IN718) is a well-known nickel-based superalloy that is extensively used in high-value-added engineering applications such as jet engines in aerospace and steam generators in nuclear power plants, as well as in the defense and marine sectors. It has excellent mechanical properties, fatigue resistance, and corrosion resistance.

IMG7215

01

Powder characteristics

Powder characteristics: high batch stability, good sphericity, low oxygen content, uniform particle size distribution, good fluidity, high bulk density and tap density.

02

Applicable processes

Powder can be used for laser/electron beam additive manufacturing (SLM/EBM), powder metallurgy (PM), laser direct deposition (DLD), powder hot isostatic pressing (HIP), metal injection molding (MIM) and other processes.

03

Applicable equipment

Powder can be used for various types of metal 3D printers, including Renishaw in the UK, EOS, ConceptLaser in Germany, SLM, 3D systems in the United States, Arcam, BLT, Farsoon, E-Plus, HBD, etc.

04

Powder application

Nickel-based metal powder is widely used in industrial and aviation turbines, petrochemicals, nuclear reactors, laser cladding and other fields.

 

 

Product Specification

 

 

Norminal Composition(wt%)

In718

Cr

Mo

Nb

Co

Fe

Al

17.0-21.0

2.8-3.3

4.75-5.5

≤1

Bal.

0.2-0.8

Ti

Si

Ni

O

N

 

0.65-1.15

≤0.35

50-55

≤500ppm

≤100ppm

 

Common Size:15-45um,15-53um,45-106um,45-150u,-200/-300/-400/-500/-600mesh etc,.

 

No

Name

Chemical Composition(wt%)

1

18Ni300

Ni17-19,Mo4.5-5.2,Co8.5-9.5,Ti0.6-0.8,Al0.05-0.15,Fe(Bal.)

2

Hastelloy Alloy

Fe17-20,Cr20.5-23,Mo8-10,W0.2-1,Co0.5-2.5,C0.05-0.15,Ni(Bal.)

3

AlSi10Mg

Si9-11,Mg0.2-0.45,Al(Bal.)

4

CoCrW

Cr26.5-29,W7-9,Si1.2-1.9,Co(Bal.)

5

Co28Cr6Mo

Cr27-29,Mo5-7,Co(Bal.)

6

Spherical Ti Powder

Ti≥99.9

7

TC4

Al5.5-6.8,V3.5-4.5,Ti(Bal.)

8

TA15

Al5.5-7.1,V0.8-2.5,Mo0.8-2,Zr1.5-2.5,Al(Bal.)

9

316L

Cr16.00-18.00, Ni10.00-14.00,Mo2.00-3.00,Fe(Bal.)

10

S136

Cr12.0-14.0,Si0.8-1.0,V0.15-0.4,C0.2-0.45,Fe(Bal.)

11

In625

Cr20-23 , Mo8-10 , Nb 3.15-4.15 , Co≤1, Fe≤1 , Ni (bal.)

12

In718

Cr17-21 , Mo2.8-3.3 , Nb 4.75-5.5 , Co≤1, Ni50-51 , Fe(Bal.)

13

Spherica WC

C3.7-4.2,W(Bal.)

14

Spherical Cr Powder

Cr≥99.9

15

Spherica Mo Powder

Mo≥99.9

16

Spherica Ta Powder

Ta≥99.9

17

Spherica W Powder

W≥99.9

 

machanical properties
 

 

Tensile Strength/MPa

1000–1100

Yield Strength/MPa

700–780

Elongation After Break/%

18–26

Tensile Strength(650℃)/MPa

1050–1180

Yield Strength(650℃)/MPa

780–860

Elongation After Break(650℃)/%

22–30

 

Product Properties

1. Appearance:Grey spherical powder

2. Tapping Density:4.89g/cm3

3. Apparent density: 4.18g/cm3

4. Flowability:18.1s/50g

5. Size: 15-53um

6. PSD: D10:23.18um, D50:35.68um, D90: 54.62um

product-669-231

 

Application

AM

Additive manufacturing

productcate-1-5

Powder metallurgy(PM)

20240619144600

Metal injection moldinb(MIM)

 

 
Our  Testing Equipment
 
20240619134653
Powder nitrogen oxygen analyzer
20240619145109
Powder Chemical Composition Tester
20240619145112

 

scanning electron microscope

 

20240619145704

 

Fluorescence Spectrometer Element Analyzer
20240619150220
Powder Laser Particle Size Tester             
20240619150323
Bulk density, tap density, flowability tester

 

 
Our factory & quipment
 
1
Powder Nitrogen Oxygen Analyzer
2
Powder Chemical Composition Tester
3
Powder Chemical Composition Tester
4
Fluorescence Spectrometer Element Analyzer
5
precision parts processing line
6
Bulk Density, Tap Density, Flowability Tester

 

 
Our factory & Office
 
1
product-496-372
3
Certifications

 

1
2
4
modular-4
5
modular-6
 

 

Our Packing
20221116114847
IMG5186
IMG1415
product-376-282

FAQ

1. Who Are We?

We are based in Hunan, China, our product sell to Asia, Europe, America, North America and Southeast Asia, and we are fully capable of undertaking global business. There are total about 101-200 people in our factory

2. How Can We Guarantee Quality?

Always a pre-production sample before mass production;

Always final Inspection before shipment;

3. What Can You Buy From Us?

3D printing metal powder ,MIM powder, Brazing powder&paste, Electronic paste, the products included are 316L,17-4ph,H13,FeSiAl,Inconel718,Inconel625, Silver based filler metal, Copper based filler metal, Nickel based filler metal, Silver paste,Rare earth products.

4. Why Should You Buy From Us Not From Other Suppliers?

Hunan Mana Materials Technology Co.,Ltd is a professional manufacture metal powder and paste .High purity rare earth series and other products etc. We have factory. We are sure we can supply the high quality products with competitve price.

5. What Services Can We Provide?

Accepted Delivery Terms: FOB,CIF,EXW,DDP,DDU,Express Delivery;

Accepted Payment Currency:USD,RMB

Accepted Payment Type: T/T,Paypal

Language Spoken:English,Chinese

 

Hot Tags: cuzn45 brazing filler metal, China, suppliers, factory, customized, price, cheap, for coating, for 3D printing, Silver Based Brazing Alloy, CuSnTi Brazing Filler Metal, CuP8 Brazing Filler Metal, Silver Based Brazing Alloy, CuSnTi Brazing Filler Metal, CuP8 Brazing Filler Metal

At present, our company integrates domestic sales and foreign trade, and has won the trust of customers with good reputation and excellent Additive manufacturing nickel-based superalloy IN718 powder GH4169 powder Inconel718 powder. We regard the fulfillment of social responsibility as "the pursuit beyond profit", and strive to build an excellent corporate image of "trusted by investors, loved by employees, respected by society, and praised by the public", and become a role model for all enterprises in society. All employees of the company will seize business opportunities with a pragmatic and innovative spirit, and seek development with a high degree of enthusiasm and high morale.

Hot Tags: inconel 718 powder, China, suppliers, factory, customized, price, cheap, for coating, for 3D printing, 18Ni300 Powder, CuSnTi Brazing Filler Metal, Silver Paste for Varistors, Silver Paste for Piezoelectric Ceramics, 17-4PH Stainless Steel Powder, Refractory Metal Powder

[[ProKeywords]]

Send Inquiry